Hard Chrome Piston Rod Range

Chrome-plated piston rods in multiple steel grades and treatment conditions.

AI-generated illustration of Hard Chrome Piston Rod Range
AI-generated illustration

Product Overview

Specify the steel grade, heat treatment, coating, diameter tolerance and end machining on the drawing. The finish values below are listed by diameter and option.

Applications and Selection

Start with the substrate grade and treatment, then choose the finish of the running surface. Different diameter ranges have their own listed straightness and coating values, so use the line that corresponds to the requested size.

For seal applications, specify the finished diameter, roughness, plated length and any nickel underlayer requirement. Confirm transitions to end machining and the allowable coating limits there.

Specifications

Steel composition by grade (wt%)

Material GradeChemical Composition (wt%)
CSiMnCrMoVP≤/S≤
45# Steel0.42–0.500.17–0.370.50–0.80–––0.040/0.040
CF530.50–0.570.15–0.350.60–0.90–––0.035/0.035
40Cr0.37–0.440.17–0.370.50–0.800.80–1.10––0.040/0.040
42CrMo0.38–0.450.17–0.370.50–0.800.90–1.200.15–0.25–0.040/0.040
16Mn0.12–0.200.20–0.551.20–1.60–––0.035/0.035
20MnV60.17–0.230.15–0.351.40–1.80––0.10–0.200.035/0.035
GCr150.95–1.050.15–0.350.25–0.451.40–1.65––0.025/0.025
60Si2Mn0.56–0.641.50–2.000.60–0.90–––0.035/0.035

Heat treatment options

Heat Treatment Condition
NormalNormal
Quenched and Tempered (Quenching + Tempering)Quench + Temper (Q+T)
Quenching (Induction Hardening)Induction Hardening
Quenched & Tempered + Quenching (Induction Hardening)QT + Induction Hardening

Induction hardening by grade

Material GradeSurface Hardness After Induction Hardening
45# SteelHRC 58 ± 3
CF53HRC > 60
40CrHRC 58 ± 3
42CrMoHRC 58 ± 3
GCr15HRC > 60
20MnV6HRC 48 ± 3

Mechanical properties before heat treatment

Material GradeMechanical Properties without Heat Treatment
Tensile Strength Rm ≥(Mpa)Yield Strength Rp0.2 ≥(Mpa)Elongation after Fracture A ≥(%)Blank Hardness (HB)
45# Steel60035516170–220
CF5363037014180–235
40Cr65040014185–230
42CrMo70045012200–245
16Mn (Q345B)470–63034521140–180
20MnV660038018165–210
GCr1565039012170–207
60Si2Mn75048010210–255

Mechanical properties after heat treatment

Material GradeMechanical Properties after Heat Treatment
Heat Treatment ConditionTensile Strength Rm (Mpa)Yield Strength Rp0.2 ≥ (Mpa)Elongation after Fracture A ≥ (%)Hardness (HB)
45# SteelQuenched and Tempered (Quenching + Tempering)650–850430–55010–15220–260
CF53Quenched and Tempered (Quenching + Tempering)700–900480–6009–14230–270
40CrQuenched and Tempered (Quenching + Tempering)800–1000600–8009–12240–280
42CrMoQuenched and Tempered (Quenching + Tempering)900–1100750–90010–15260–300
16Mn (Q345B)Normalizing / Hot Rolling470–63034521140–180
20MnV6Quenched and Tempered (Quenching + Tempering)700–900500–70012–16200–250
GCr15Spheroidizing Annealing / Quenched and Tempered800–1000550–7008–12190–230
60Si2MnQuenched and Tempered (Quenching + Tempering)900–1100700–9006–10240–280

Surface treatments

Surface Treatment MethodChrome Plating
Nickel Plating
Nickel Plating + Chrome Plating
Laser Cladding
HVOF
Nitriding

Diameter, finish and tolerance

Diameter RangeStraightnessChrome ThicknessNickel ThicknessStandard LengthChrome Layer HardnessDiameter ToleranceRoundnessSurface Roughness
3<Ø≤250.15 mm/mØ≤25 mm: Min 15 µmØ≤25 mm: Min 10 µm2 m, 3 mHV 850–1050High Precision: g6, h6 Standard: f7, f8, h7, h8≤ 1/2 Diameter ToleranceRa ≤ 0.2 µm
25<Ø≤400.10 mm/mØ>25 mm:Min 20 µmØ>25 mm:Min 15 µm3 m, 6 m, 7.5 m
40<Ø≤800.10 mm/m
80<Ø≤1500.05 mm/m
150<Ø≤2000.05 mm/m
200<Ø≤3000.05 mm/m
Ø>3000.05 mm/m