Wuxi, Jiangsu, China yangxin0916@sina.com +86 510 8369 0197 EN 中文

Piston Rod Materials and Heat Treatment

The original technical guide discusses 45# steel, 40Cr and 2Cr13. These materials respond differently to quenching, tempering and surface hardening.

Material and treatment should follow part geometry, service load and wear or corrosion requirements. Specify whether a hardness requirement applies to the core or the surface, and identify where it should be measured.

Call Out Material, Heat Treatment and Surface Finish Separately

Start with the required steel grade and delivery condition. A core mechanical-property requirement and a surface hardness requirement describe different parts of the rod. State the measurement location and method where these are defined.

If a wear surface is induction hardened, mark the treated length and the required case depth on the drawing. List hard chrome and final grinding separately if the design also calls for them.

Project enquiries

Working from a drawing?

Send the critical dimensions, finish and quantity. We’ll help you check the right product family.

Request a Quote