Product Overview
Specify finished diameter, fit, straightness and surface roughness for precision shaft and locating applications.
Applications and Selection
430 is a ferritic grade. If the project specifies it, verify the grade on the purchase request and review the actual exposure conditions and finish needed for the component.
When an outside diameter will serve as a guide surface, mark the fit and roughness separately from dimensions that will be machined after delivery.
Specifications
Material identification
| Item | Technical Parameters |
|---|---|
| Material Grade | 430 |
| Chinese National Standard Grade | 10Cr17 |
| UNS Grade | S43000 |
| DIN Grade | 1.4016 |
Chemical composition (wt%)
| C | Si | Mn | P | S | Cr |
|---|---|---|---|---|---|
| ≤0.12 | ≤1.00 | ≤1.00 | ≤0.040 | ≤0.030 | 16.00–18.00 |
Mechanical properties
| Item | Mechanical Properties |
|---|---|
| Tensile Strength Rm | ≥450 MPa |
| Yield Strength Rp0.2 | ≥205 MPa |
| Elongation after Fracture A | ≥22% |
| Brinell Hardness | ≤183 HB |
Dimensions and precision
| Item | Technical Requirements |
|---|---|
| Common Diameter Range | Ø3.0 mm – Ø300 mm |
| Diameter Tolerance | Standard grade: h8, h9; High-precision grade: h7, f7, g6, h6 |
| Roundness | ≤1/2 of diameter tolerance |
| Straightness | ≤0.10 mm/1000 mm |
| Standard Length | Ø40 mm and below: 3 meters; Over Ø40 mm: 6 meters available (custom fixed lengths acceptable) |
| End Face Requirements | Flat ends, chamfered and deburred |
Processing and surface finish
| Process Type | Complete Process Flow | Surface Roughness |
|---|---|---|
| Process 1 | Hot-rolled base material → Precision drawing → Centerless precision grinding | Ra 0.4–0.8 µm |
| Process 2 | Hot-rolled base material → Peeling & straightening → Centerless precision grinding | Ra 0.4–0.8 µm |
| Process 3 | Hot-rolled base material → Peeling & straightening → Centerless precision grinding → Polishing | Ra ≤0.2 µm |