Product Overview
Select coating thickness, finished outside diameter and tolerances to match the application drawing.
Applications and Selection
For a loaded shaft, confirm the 431 substrate condition independently of the working chrome surface. The product tables list different quenched and tempered conditions, so match the one called out on the drawing.
Identify the relevant strength condition, chrome thickness and the datum for straightness or runout. Provide the working section length and end connection details.
Specifications
Finish and dimensional requirements
| Item | Technical Parameters |
|---|---|
| Base Material Grade | 431 |
| Chinese National Standard Grade | 17Cr16Ni2 (1Cr17Ni2) |
| UNS Grade | S43100 |
| DIN Grade | 1.4057 |
| Surface Treatment | Chrome Plated |
| Hard chrome thickness | Diameter ≤Ø20: 15 µm; Diameter>Ø20: 20 µm, thickness customizable on demand |
| Surface Hardness after Chrome Plated | HV800–1100 |
| Common Diameter Range | Ø3.0 mm–Ø300 mm |
| Diameter Tolerance | Standard: h8, h9; High Precision: h7, f7, g6, h6 |
| Roundness | ≤1/2 diameter tolerance |
| Straightness | ≤0.10 mm/1000 mm |
| Standard Length | Fixed length of 3 meters for Ø40 mm and below; fixed length of 6 meters for diameters above Ø40 mm, customized fixed lengths available for large specifications |
| End Face Requirements | Flat ends, chamfered and deburred |
Base material composition (wt%)
| C | Si | Mn | P | S | Cr | Ni |
|---|---|---|---|---|---|---|
| ≤0.20 | ≤1.00 | ≤1.00 | ≤0.040 | ≤0.030 | 15.00–17.00 | 1.50–2.50 |
Base material mechanical properties
| Item | Mechanical Properties |
|---|---|
| Tensile Strength Rm | ≥860 MPa |
| Yield Strength Rp0.2 | ≥655 MPa |
| Elongation after Fracture A | ≥15% |
| Base Material Hardness | 260–300 HB |
Quenched and tempered mechanical properties
| Quenching and Tempering | QT800 | QT900 |
|---|---|---|
| Tensile Strength Rm ( MPa) | 800–950 | 900–1050 |
| Yield Strength Rp0.2 ( MPa) | ≥600 | ≥700 |
| Elongation after Fracture A5 (%) | ≥13 | ≥12 |
| Room-temperature Impact Energy KV₂ (J) | ≥25 | ≥20 |
| Brinell Hardness HB | 240–290 | 270–320 |
| Rockwell Hardness HRC | 23–30 | 27–35 |
Processing and surface finish
| Process Type | Complete Process Flow | Surface Roughness |
|---|---|---|
| Process 1 | Hot-rolled base material → Precision drawing → Centerless precision grinding → Polishing → Chrome Plated → Polishing | Ra ≤0.2 µm |
| Process 2 | Hot-rolled base material → Peeling and straightening → Centerless precision grinding → Polishing → Chrome Plated → Polishing | Ra ≤0.2 µm |
| Process 3 | Forged round bar → Turning finishing → Centerless precision grinding → Polishing → Chrome Plated → Polishing | Ra ≤0.2 µm |