Specifications
Finish and dimensional requirements
| Item | Mechanical Properties |
|---|---|
| Substrate Grade | 316L |
| National Standard Grade | 022Cr17Ni12Mo2 |
| Surface Treatment | Chrome Plated |
| Hard chrome thickness | Diameter ≤Ø20: 15 µm; Diameter >Ø20: 20 µm, thickness customizable as required |
| Surface Hardness after Chrome Plated | HV800–1100 |
| Common Diameter Range | Ø3.0 mm–Ø300 mm |
| Diameter Tolerance | Conventional: h8, h9; High Precision: h7, f7, g6, h6 |
| Roundness | ≤1/2 diameter tolerance |
| Straightness | ≤0.10 mm/1000 mm |
| Standard Length | Fixed length of 3 meters for Ø40 mm and below; fixed length of 6 meters for above Ø40 mm, customized fixed lengths available for large specifications |
| End Face Requirements | Flat end, chamfered and deburred |
Base material composition (wt%)
| C | Si | Mn | P | S | Cr | Ni | Mo |
|---|---|---|---|---|---|---|---|
| ≤0.03 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 16.00–18.50 | 10.00–14.00 | 2.00–3.00 |
Base material mechanical properties
| Item | Index Requirements |
|---|---|
| Tensile Strength Rm | ≥485 MPa |
| Yield Strength Rp0.2 | ≥175 MPa |
| Elongation after Fracture A | ≥40% |
| Substrate Hardness | ≤187 HB |
Processing and surface finish
| Process Type | Complete Process Flow | Surface Roughness |
|---|---|---|
| Process 1 | Hot-rolled substrate → Precision drawing → Centerless precision grinding → Polishing → Chrome Plated → Polishing | Ra ≤0.2 µm |
| Process 2 | Hot-rolled substrate → Peeling and straightening → Centerless precision grinding → Polishing → Chrome Plated → Polishing | Ra ≤0.2 µm |
| Process 3 | Forged round bar → Turning finishing → Centerless precision grinding → Polishing → Chrome Plated → Polishing | Ra ≤0.2 µm |